    To all. I am in the process of typing up a 3 month review of my experiences with Everlast and the purchase of a powerpro256 and a power I-MIG 250p. Stay tuned in the next few days for the review.

  2. #2

    Cool review

    Come on, don't leave us hangin.

  3. #3

    Default

    A 250 amp AC/DC TIG, 60 amp plasma cutter and a 250 amp MIG with pulse.

    I work for Everlast and have that for personal use.

    My 250P was used for 4 hours today (jeep racing seat brackets) on my day off. And my Power Plasma 60 was used yesterday to cut all the parts (and today to cut the parts I forgot). I can't imagine anyone that would not like that combo.

    I agree Powercat, even I was waiting for the results expecting something was up actually. But this time of the year, people are busy, so maybe the delay?

    Hope we see the review soon too.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Question review

    Still waiting.

  5. #5

    Default

    Wow. Still nothing but crickets in here...

  6. #6

    Default

    Zoomie,

    Too bad this thread did not get wiped in the database conversion, rather than all the nice project threads.

    Will manually kill it soon if nothing shows up.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    As useless as it is, the moment you delete it someone will say that it was removed due to a negative review. "damned if you do, damned if you don't" it seems...

  8. #8

    Default

    Zoomie,

    That's true, but this is the Everlast Support Welding forum and we can delete a thread if it serves no purpose or a case is resolved for an unhappy customer that chose to post rather than pick up a phone. I still think the Miles' thread is still out there (and he actually posted we can remove it months ago and he was happy now) and it will get removed at some point.

    No matter how much fake bad press we get on some sites, people still buy our units. So that's not really a concern for us. Our customers know we are the real deal and they spread the word. I wish we could keep up with the demand, rather getting posts that people are waiting on units. But that does say something if we can not build them fast enough.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. 5 month old PowerTig 250EX and heres what I think
    By Gustaf in forum Customer Testimonials
    Replies: 0
    Last Post: 04-23-2018, 05:30 PM
  2. Been waiting over a month for everlast canada to get more plasma cutters in stock
    By dabooge in forum Pre-sales, Sales and Shipping questions
    Replies: 0
    Last Post: 10-15-2014, 02:51 PM
  3. Review of my new I-MIG 200.
    By 225 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 9
    Last Post: 03-10-2013, 08:42 PM
  4. Technical support call of the day, well the week or the month at least
    By performance in forum Technical Bulletins and Tips
    Replies: 0
    Last Post: 09-27-2012, 06:31 PM
  5. Super Cut 50 Review
    By WAYNESWORLD in forum Everlast Plasma Cutters (PAC)
    Replies: 17
    Last Post: 12-28-2009, 04:54 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •