    Default 2nd BMX Build

    This is my second BMX frame. For fun I thought I would use tubemitre.exe. It was very simple to use and I will not hesitate to use it again. Tubemitre.exe would be great for larger diameter fishmouths.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	gh bmx and welder.jpg 
Views:	1213 
Size:	67.6 KB 
ID:	680  

  2. #2

    Default

    I downloaded tubemitre, I have been looking for a program like that for years,
    You can buy the templates at welding shops but now I can make my own templates, cool program for the fabricator to have on hand. I hope Santa brings you a cart for that nice machine you keep on the floor.

  3. #3

    Default

    A cart might be handy, I have something in my shed I am concidering. Its a retail rack on castors, about 2' square and the top rack is at about 4'. The thing is I do most of my work on the road, repairing wine tanks and commercial kitchens. But how awesome is that machine? I'm up in Canada and its cold. I thought it might mess with the sensitive electronics. Not even close, smooth every time and the settings are exactly where I left them with pedictable results every time I start the machine.

  4. #4

    Default

    You may want to try Tube Bender from JD2 at
    http://www.jd2.com/shop/custom.aspx?recid=9
    for free software to bend tubes and design.

    For those that need a cool tool for tube notching
    That tubemite program can be found at http://www.ozhpv.org.au/resources/shed/tubemiter.html

  5. #5

    Default

    I have that tube bend program, I am still learning it, its cool to animate your bends. On topic of bending tube, I have a problem with wrinkling tubes. I am bending 5/8" .035 4130, 3/4 .035 4130, and 7/8 .035 4130. I would like to do these bends around the smallest die possible and keep it clean. Any suggestions?

  6. #6

    Default

    I'm getting ready to order a set of tubes for a road bike. Do you build with a jig? I've built hand rails and roll cages in the past, but I'm a little unsure how to keep everything aligned.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  7. #7

    Default

    what size gas cyclinder is that? looks like s streach model
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  8. #8
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Did you purchase the tubes for the tubes for the front end and the pedals to accept the bearings? That would be a cool project to do for the kids.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  9. #9

    Default

    I hope you have that argon tank secure if it falls over and knock the valve off it could be ugly

  10. #10

    Default

    Quote Originally Posted by DVA View Post
    Did you purchase the tubes for the tubes for the front end and the pedals to accept the bearings? That would be a cool project to do for the kids.
    Quote Originally Posted by 67cudafb View Post
    I hope you have that argon tank secure if it falls over and knock the valve off it could be ugly
    The person who started this thread hasn't been active here in a year.
    Always look at the thread date and if it's an old one, click on the member's name and then "view forum posts" to see if they're still active.
    Last edited by zoama; 10-10-2011 at 12:13 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  11. #11

    Default

    Quote Originally Posted by zoama585 View Post
    The person who started this thread hasn't been active here in a year.
    Always look at the thread date and if it's an old one, click on the member's name and then "view forum posts" to see if they're still active.
    this isnt the first time you have said the exact same thing, why are dead posts coming back to life? zombies?
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  12. #12

    Default

    Quote Originally Posted by jerky View Post
    this isnt the first time you have said the exact same thing, why are dead posts coming back to life? zombies?
    Nah just new members looking at interesting threads and not noticing the date. People have all different levels of internet experience just like welders have all different levels of welding experience.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Bumper build questions
    By Vanman in forum General Welder Questions
    Replies: 6
    Last Post: 08-07-2014, 12:09 AM
  2. Pig roaster and bbq grill build
    By melman680 in forum Other Custom Fabrications
    Replies: 3
    Last Post: 06-02-2014, 03:25 AM
  3. Cart Build
    By its_34 in forum Other Custom Fabrications
    Replies: 55
    Last Post: 12-16-2013, 12:47 PM
  4. KTM SMR Build.
    By 225 in forum Truck, Car and Bike builds
    Replies: 11
    Last Post: 12-06-2012, 07:02 PM
  5. Tigging and my build
    By Mad-Dax in forum On Road Fabrication
    Replies: 5
    Last Post: 04-13-2012, 04:27 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •