Nice looking welds. This is the type of material for which I am looking into a tig to weld. I just need to decide on either the PowerTig or the PowerPro.
dont know about nice looking welds but maybe a start in the right direction ....
you need to get some penetration on the toes of those welds they are COLD weld being only on the surface of the base material
weld it HOT and Fast its not steel