I tried both the standard collet body and a gas lens on the 20 torch I bought here in Canada and neither seemed to give gas coverage. Hooked up the big 17 and it worked fine.
Chuck
I tried both the standard collet body and a gas lens on the 20 torch I bought here in Canada and neither seemed to give gas coverage. Hooked up the big 17 and it worked fine.
Chuck