  1. Default Cart before the horse

    I purchased a Weldmark 24W-25 foot 180 amp water cooled TIG torch. No welder yet.<G>.
    Now I can't locate any consumables for the durn thing. Not even Chinese.
    The Weldmark site is one big mess and ebay has no listing for the '24'.
    I thunk I got meself a big yellow lemon.. . .charlie

  2. #2

    Default

    A 24 is a micro torch. It has no back cap and the consumables are real short. Its made for getting into tight spaces, behind pipes close to walls and floors and similar applications. I have a torch body myself. About any welding supply store should have the consumables....No problem. Just look for it under WP24 (weldcraft).

  3. Default

    Would it be possible to attach a different torch to the cable, gas and water lines?

  4. #4

    Default

    Can you clarify your statement? What different torch to what cable? what gas?...etc?

  5. Default

    Performance. . . . I would like to salvage the water hoses, the gas hose and the conductor cable and put a 'regular' torch head on these. This should be possible, hopefully. Do you know where I can locate consumables online for the 24W?

  6. #6

    Default

    Here are parts and consumables for the wp24.
    http://www.arc-zone.com/index.php?ma..._727_20_48_210

    Are you sure that this is what you bought? In your original post you said you had a 180amp water cooled torch. The wp24 is a 80amp air cooled torch.
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

  7. #7
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Slip the handle off the torch head, and you will see connectors under the handle where the cables connect with the torch head. Just get a replacement torch head that matches the connectors on your cables, and the torch head should be a direct swap.

    Be careful not to exceed the current carrying capability of your leads, or you can melt the insulation. (Which is really bad news; see pic for a one-piece aircooled hose that got melted from exceeding the cable's current&duty cycle.)

    Weldcraft shows the same part numbers for the gas, water, and power hoses of the WP-24W as they show for the WP-20, so you should be able to swap a WP-20 torch head onto those WP-24 cables.
    http://www.weldcraft.com/pdfs/WP24ENG_1.pdf
    http://www.weldcraft.com/pdfs/WP20ENG.pdf
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	melted_cable_inside_1.JPG 
Views:	389 
Size:	105.1 KB 
ID:	824  
    Last edited by jakeru; 02-20-2011 at 06:54 PM.

  8. Default

    Jakeru . . . . thanks so much for the assistance. . .charlie

  9. Default

    The torch and hoses I purchased are WELDMARK, not Weldcraft. Mine is the 24W-25. It is listed as 180 amps. I'm having a heck of a time locating comsumables for this small torch. In Jodys videos he said he liked a smaller torch and was going to get a #7. Any idea of what brand and part number for this torch?

  10. #10

    Default

    Footboarder,

    Don't worry about who makes it. Weldcraft is the standard that almost all torches are made to. Whethere its Everlast, weldtech, weldstone, weldmark,weldcraft, CK or others, everybody uses the same basic design and nomenclature such as wp 18, wp 17, wp, 26, wp 24 etc. Some may have an extra letter or number, but nearly all will be almost identical in construction. Consumables will interchange pretty easily from brand to brand, as they use the same threads, and dimensions. Yours should easily interchange with any weldcraft or other brand 24 series torch. It isn't as common as some, but it isn't uncommon either.

Similar Threads

  1. Al Horse trailer
    By robt in forum General Welding Questions
    Replies: 3
    Last Post: 03-01-2015, 07:48 PM
  2. Welding Cart - Power Cart 250 - opinions?
    By ScottRussell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 12-05-2012, 01:19 PM
  3. Replies: 15
    Last Post: 08-02-2012, 01:30 PM
  4. Oxy/Ac weld aluminum for a horse stand
    By beezfun in forum General Welding Questions
    Replies: 7
    Last Post: 08-28-2011, 08:27 PM
  5. Horse Stall Door Sign
    By cpierce18 in forum Personal Projects (no welder required)
    Replies: 3
    Last Post: 07-06-2011, 04:29 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •