Share
Results 1 to 2 of 2

Thread: NO HF arc start on my CT520

  1. Default NO HF arc start on my CT520

    My CT520 suddenly lost its HF arc start, I've been scratch starting it on TIG, but this is really shortening the tungsten electrode resharpening time. Any suggestions on how to fix the HF circuit? The manual that came with this unit is useless and almost unreadable. I don't want to start monkeying around inside this unit without some guidance and diagrams. Is there a HF circuit board that can just be replaced?
    Thanks Jon C.

  2. Default Re: NO HF arc start on my CT520

    Jon,

    Did you try the HF adjust instructions here?

    If you can PM me your phone number and I can call you and walk you though it.
    Mike R.
    http://www.everlastwelders.com
    http://www.everlastgenerators.com

Similar Threads

  1. CT520 Plasma cutter consumables
    By cardoc in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 11-01-2012, 12:54 PM
  2. Off to a bad start...
    By WitchHunter in forum Pre-sales, Sales and Shipping questions
    Replies: 4
    Last Post: 05-30-2012, 08:58 PM
  3. CT520 broke down
    By Martygras in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 04-22-2011, 10:43 PM
  4. intermit pilot arc with CT520
    By cardoc in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 10
    Last Post: 01-20-2011, 01:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •