Originally Posted by
cmd
I got it last week. Its probably 12 feet. I have a 25' torch. I think it was $35 total for the switch. I hadn't gotten to use it much, (with new switch) last night I used it a bit and it works very nice. The paddle comes with 2 or 3 connectors but none of them fit my EX so I just chopped the one off the old torch. I would like to buy some extras some where if someone knows the common name of that connector.
Is this the switch they sent you?
http://www.everlastgenerators.com/products1/409_1.jpg
That one shows 15.99 on this sight.
Here is the 7 pin connectors.
http://cgi.ebay.com/7-pin-connector-...#ht_2070wt_905
Looks like they should work. I ordered them last night.
Gerald