    Due to me despising the factory torch on the EX I finally went and go a new one. Before I hear how great and ergonomic the original torch was I understand but it was had some hold backs for me.
    torch too big.
    cables too heavy
    cables too short
    cables too stiff
    torch leaked water from the fittings inside, maybe my miller watermate had to much pressure, I took it apart, nothing you could do just too much pressure. So I went to my LWS which is stocked with good people and they set me up with this rig. this torch is a WP20 size ESAB, it is rated 250 amp DC and 240 amp AC according to its spec sheet.
    I don't know what some of these adaptors are called but there is a really nice adapter they found to attach the screw on power cable to the dinse as you can see. Also their water cooler quick connects fit the argon quick connect on the EX without leaking, but it has LH thread so they made me a short hose to go from RH thread argon to the LH water thread in the make quick connect. I then got the leather sheath which was a must. I am very satisfied with this unit now and am much more efficient with this new torch. I called Alex and they are sending me a new paddle type switch for the torch then I'll be done. Photos follow.
    chris









  2. #2

    Default

    How much do have tied up in the new torch and the adapters to convert it to fit?
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

  3. #3

    Default

    grand total with collets, ceramics, and all the misc. stuff I was about $300 after tax, I think their was some adapters I may not have paid for as they just had them laying around. I like how high this torch is rated on the amperage compared to some other 20's. the leather sheath is around $2 a foot and I have like 23 feet for a 25 foot torch lead. I just went local so I could just be done with it instead of trying to buy parts online and match things up for a month.

  4. #4

    Default

    Was wondering if you got your torch switch from Alex yet? Was wanting to know how long the lead is on it. Since you now have a 25' torch lead (at least it appears that way), I'm thinking the lead on the Everlast switch will be to short. I guess it would be simple enough to lengthen, as it only uses two wires on the 7 pin socket.
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

  5. #5

    Default

    I got it last week. Its probably 12 feet. I have a 25' torch. I think it was $35 total for the switch. I hadn't gotten to use it much, (with new switch) last night I used it a bit and it works very nice. The paddle comes with 2 or 3 connectors but none of them fit my EX so I just chopped the one off the old torch. I would like to buy some extras some where if someone knows the common name of that connector.

  6. #6

    Default

    7 pin panasonic

    Someone posted a link to them real cheap last night on ebay.

  7. #7

    Default

    Quote Originally Posted by cmd View Post
    I got it last week. Its probably 12 feet. I have a 25' torch. I think it was $35 total for the switch. I hadn't gotten to use it much, (with new switch) last night I used it a bit and it works very nice. The paddle comes with 2 or 3 connectors but none of them fit my EX so I just chopped the one off the old torch. I would like to buy some extras some where if someone knows the common name of that connector.
    Is this the switch they sent you?
    http://www.everlastgenerators.com/products1/409_1.jpg
    That one shows 15.99 on this sight.

    Here is the 7 pin connectors.
    http://cgi.ebay.com/7-pin-connector-...#ht_2070wt_905
    Looks like they should work. I ordered them last night.
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

Similar Threads

  1. AMPTroll torch for my 250ex machine needed.
    By will in forum TIG Welding (GTAW/GTAW-P)
    Replies: 15
    Last Post: 11-19-2015, 10:37 PM
  2. 250ex stock torch mods.
    By Scotty1 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 06-18-2012, 10:17 AM
  3. For those who decide to add a new torch to the Powertig 250EX........
    By Steve in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 09-04-2011, 02:18 AM
  4. CK 200 Torch to 250EX with Photos and Part #'s
    By Rugar in forum TIG Welding (GTAW/GTAW-P)
    Replies: 34
    Last Post: 08-18-2011, 09:18 PM
  5. Foot Pedal and Torch on 250EX
    By Rugar in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 08-01-2010, 06:13 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •