    Just a quick post too let Everlast know I am very pleased with my new PowerArc 200 inverter I have used this for about a week now and can find no faults! Lots of power for a great price!
    including a picture of 1st pass on a fillet weld done today on 1/2" to 1" plate,5/32 7018 at 165 amps EP
    Regards Bob


    wide weave cover 1/8 ,7024 ,140 amp, en

    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	100_6027PowerArc1 (Small).jpg 
Views:	38879 
Size:	57.8 KB 
ID:	520   Click image for larger version. 

Name:	wide weave (Custom).jpg 
Views:	9034 
Size:	42.3 KB 
ID:	521  
    Last edited by Doxie; 09-22-2010 at 06:55 PM. Reason: Pict
    Trermal Arc T-Bird 270 Amp gas welder gen
    Thermal Arc Pro Wave 185
    PowerArc 200
    power Imig 205
    SM 200-N mig spool gun
    Riland 60 Plasma
    HF 40 Plasma
    ReadyWelder II
    180 Amp Diesel Welder Gen
    Henrob Torch
    Arcair K4000
    2 Ox-Aect outfits

Similar Threads

  1. 250EX Rocks!
    By Twisted Z in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 11-25-2015, 05:09 AM
  2. PowerArc 300
    By Shield Arc in forum Stick Welding (SMAW)
    Replies: 6
    Last Post: 11-19-2014, 12:28 PM
  3. Powerarc 140 on 208 vac
    By daverepair in forum Stick Welding (SMAW)
    Replies: 18
    Last Post: 05-16-2012, 04:24 AM
  4. New PowerArc 200
    By Tasha71822 in forum Customer Testimonials
    Replies: 6
    Last Post: 11-05-2011, 11:21 PM
  5. everlast rocks
    By onlyellis in forum Introduce Yourself
    Replies: 1
    Last Post: 11-04-2008, 12:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •