  1. Default ACDC 200 tig Argon Questions

    Does any one have a ACDC 200 pulsed?
    What do you set the argon flowmeter to for mild steel 120 amps?
    Is there a rule of thumb for this?

  2. #2
    Join Date
    Mar 2011
    Location
    mission viejo CA
    Posts
    92

    Default

    10-20 cfh i would run it at 12-14
    Lincoln precision tig 275
    Miller Syncrowave 350 Tig
    Miller 250 Mig
    old miller 200 Mig
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list

Similar Threads

  1. 2 simple questions about argon and filler rod
    By JohnT in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 08-08-2014, 06:34 PM
  2. PA 160sth..CAN YOU RUN ON DC/ACDC GENERATOR
    By stretch in forum Stick Welding (SMAW)
    Replies: 7
    Last Post: 03-05-2014, 11:41 AM
  3. NEW 2013 EVERLAST PowerTIG 185 ACDC TIG / STICK WELDER
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 23
    Last Post: 12-24-2012, 12:43 AM
  4. Argon gauge questions/ball type flow meter
    By Longlasting in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 13
    Last Post: 07-07-2010, 06:00 AM
  5. Purchased 200 ACDC Pulsed
    By wallnut in forum Customer Testimonials
    Replies: 2
    Last Post: 05-01-2009, 12:54 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •