  1. Default

    It looks as if the tungston is being contaminated in some of the pics .

    On a side note is the backside of the material clean also ?

    What are you welding on top of steel table ? plywood ? In the last pic it looks to me what ever is under the two pieces is where the problem is.

    What is your argon flow rate and you are using your machine in AC correct ?
    Jake
    Last edited by jakesporting; 09-06-2010 at 03:50 AM.

Similar Threads

  1. 200dv low ampegare dc tig welding issue
    By 200dx in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 09-13-2016, 04:32 AM
  2. My new MTS 200 is great, BUT issue mig welding...
    By Red Rider in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 8
    Last Post: 08-08-2014, 04:35 PM
  3. 250DX AC Aluminum Weld Issue
    By dmost in forum TIG Welding (GTAW/GTAW-P)
    Replies: 58
    Last Post: 11-30-2013, 08:04 PM
  4. Replies: 2
    Last Post: 08-03-2011, 04:50 PM
  5. non-welder problem, aluminum tube joint issue
    By cmd in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 09-06-2010, 03:29 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •