Hey guys!
I just started with my new tig welder this week. Iv been working on figuring out what im doing wrong. I cant seem to pinpoint it. Im cleaning the Aluminum with acetone and a stainless steel brush before welding. I have a good ground, 2% ce tungsten(3/32), and have tried a multitude of settings. High/low freq, more and less ep/en time with no luck. I was having some trouble with the amp's and the foot pedal, but that was resolved with time behind the torch.
What I cannot figure out; im having the puddle turn into a skinned ball, im assuming its oxidized aluminum, either when the puddle is 1st formed or as soon as I touch the filler to the puddle. The ball tends to stick to the filler rod when I pull it out, or it just sits where I leave it and its very hard to melt. I have attached some pictures for everyone to see. Any help would be appreciated, its driving me nuts!
Another issue im having, when trying to join 2 thinner pieces of aluminum they just peel back from one another. I thought this was from dirty base material but I cleaned it several times and am not sure...
![]()








Reply With Quote