    I have the 250ex just so everyone knows, so far so good on that end. However, I just got done welding the structural parts of 3 ramps for ATV's/lawmowers. The long side rails are 2X2" square alum tube. the cross bars are 1" square tube. So when I weld the cross bars in between the side rails I have 8 welds on each tube, the small cross tube is eventually sealed pretty much air tight when done (against the bigger tube). I can weld about 6 out of 8 joints then it gets very hard, nearly impossible, to weld the last one or two. I think the tube is heating up and the air inside is expanding and coming out the crack I am welding on. I turned up the argon to no avail. I can't really back purge the tube either. Does this sound like a reasonable problem and does anyone have any ideas on how to get around it. I may spoolgun the next time as its pretty time consuming with the tig, maybe that will help.
    Chris

  2. #2
    Join Date
    Jul 2010
    Location
    In the Land of CoRn
    Posts
    69

    Default

    Drill a relief hole

  3. #3

    Default

    Quote Originally Posted by Slick View Post
    Drill a relief hole
    I considered this, would you go back and weld the hole shut or just let it open, are we talking 1/8" or 1/4" hole? the 1" tube is 12" long.
    chris

  4. #4
    Join Date
    Jul 2010
    Location
    Port Saint Lucie , Florida
    Posts
    85

    Default

    CMD ,
    you could just drill the hole in the 2x2 inside where the 1 x1 will be welded on then that would vent there.
    It would just need to be .125 hole.
    Gary

Similar Threads

  1. Replies: 3
    Last Post: 01-22-2016, 03:25 AM
  2. 250DX AC Aluminum Weld Issue
    By dmost in forum TIG Welding (GTAW/GTAW-P)
    Replies: 58
    Last Post: 11-30-2013, 07:04 PM
  3. Replies: 0
    Last Post: 11-15-2011, 11:55 PM
  4. Replies: 11
    Last Post: 06-24-2011, 04:51 AM
  5. New to Aluminum welding. Need some help with an issue
    By Krookz in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 09-21-2010, 06:05 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •