Pros:
Light 50 lbs or so.
Pulsed lots of dials.
Digital readout.
Low amps I think I will make an extension cord.
Worked without issue so far.
Big Metal foot pedal you can adjust the max amps on. (Very Happy)
(I thought it would vary the entire range this is a nice feature)
Very Bright Yellow hard to trip over. I think they need to put a smiley face on them.
Did not cost 3000 dollars.
Cons:
Knob to adjust max amps controlled by foot pedal is on the foot pedal.
Giant Tig torch handle.
Kind of cheesy packing (mine arrived ok though)
Ground lead sort of short.
One of the tiny screws that hold on the torch control socket was in the bottom of the torch bag. Lucky I saw it easy fix.
Manual needs a tech writer bad.
Suggestions:
Does not come with 1/4 inch hose or clamps. (Argon to welder)
I had some lying around for some reason.
Would be nice if max amps knob limited foot pedal.
Send a sharp 3/32 electrode and mild steel tig rod so you test right away.
Impressions:
So far worked like its supposed to. More to follow.
Need to get my buddy the welder to come over and test.




Reply With Quote