    Default Welding Table @ Work

    I built this welding table the second week at my new job since they brought me in as their new and first fabricator. The frame of the table I took the idea from one of the welding project pics on Miller's site and added my own little twist with the plasma cutting grate. This picture is just after finishing up the basic welding, but I've since painted the frame, and added a few more tool holding brackets and other details. I'm waiting on a catch pan to be bent up locally which I'll put under the plasma grate and be quickly removable to empty when needed.

    The table was mig welded with my Lincoln 175 hiding behind the PowerPro205, but I did use the Everlast to cut out the 18 x 21" opening. Our 30amp breaker kept tripping from extended use at 45+ amps so I had to do short 1.5" sections and keep taking breaks.

    Specs of the table are:
    4x8', 1/2" thick top sheet
    2x2", 3/16" wall square tubing
    3" non-marking casters, overall height of 5.5" (if I recall right) with locking wheel and swivel
    total weight approximately 750-800lbs. Raw materials weighed in at 850 or so on invoice, before cutting out 18x21 plate.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG955155.jpg 
Views:	873 
Size:	61.6 KB 
ID:	494  

Similar Threads

  1. NOt welding related but some of my recent hat work
    By ironmanjay in forum Other Custom Fabrications
    Replies: 10
    Last Post: 06-07-2013, 11:34 AM
  2. Grounding the work table
    By CraigJ in forum General Welder Questions
    Replies: 52
    Last Post: 06-06-2012, 06:47 AM
  3. Looking for a TIG/Plasma that would work on a CNC table as well.
    By Tacoma747 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 04-12-2012, 07:19 PM
  4. welding/ machine work I know there is a better way.
    By ScratchStart in forum Heavy Equipment and Commercial Projects
    Replies: 8
    Last Post: 04-26-2011, 03:19 PM
  5. PP256 Work table/cart
    By dirtyfarmer in forum Other Custom Fabrications
    Replies: 7
    Last Post: 06-25-2010, 12:52 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •