    Just a quick post too let Everlast know I am very pleased with my new PowerArc 200 inverter I have used this for about a week now and can find no faults! Lots of power for a great price!
    including a picture of 1st pass on a fillet weld done today on 1/2" to 1" plate,5/32 7018 at 165 amps EP
    Regards Bob


    wide weave cover 1/8 ,7024 ,140 amp, en

    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	100_6027PowerArc1 (Small).jpg 
Views:	38881 
Size:	57.8 KB 
ID:	520   Click image for larger version. 

Name:	wide weave (Custom).jpg 
Views:	9038 
Size:	42.3 KB 
ID:	521  
    Last edited by Doxie; 09-22-2010 at 06:55 PM. Reason: Pict
    Trermal Arc T-Bird 270 Amp gas welder gen
    Thermal Arc Pro Wave 185
    PowerArc 200
    power Imig 205
    SM 200-N mig spool gun
    Riland 60 Plasma
    HF 40 Plasma
    ReadyWelder II
    180 Amp Diesel Welder Gen
    Henrob Torch
    Arcair K4000
    2 Ox-Aect outfits

  2. #2

    Default

    I tried to tell people this earlier in some of my posting, now you are showing them, it is a great welder. Very reasonably priced and power to spare.

  3. #3

    Default

    This might be the next thing I get from them, I like the small package and the price, if they had one in stock when I got my plasma I might have just grabbed one then, I'll have to see, I hate to haul my 250ex all over the place, I hate for it to get damaged. Looks like it welds good, hows it do overhead and vertical up? is the 6010 thing as neat as I am told? my 250 so far has burned those (6010/11) great although it wasn't apparently designed for it.

  4. Default

    Doxie
    Glad to see your up and running . I still have not had the chance to get out to do a bit of fishing .

    I can not really answer the overhead . But i had a Customer in today and he specifically wanted to try out the vertical up weld and after burning a couple of rods in 6011 and 7014 he was very pleased with the performance
    cheers
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  5. Default First pass thickness.

    Quote Originally Posted by Doxie View Post
    Just a quick post too let Everlast know I am very pleased with my new PowerArc 200 inverter I have used this for about a week now and can find no faults! Lots of power for a great price!
    including a picture of 1st pass on a fillet weld done today on 1/2" to 1" plate,5/32 7018 at 165 amps EP
    Regards Bob


    wide weave cover 1/8 ,7024 ,140 amp, en

    Is this typical of the first pass thickness you can weld with the Power Arc 200?

  6. #6

    Default

    to answer your question about over head and v^ all though i dont have a 200 i have the 160. it works perfect and as far as the 6010 port it worked great while doing root's
    Aaron

  7. #7

    Default

    Davy,
    Yes, this is typical, though I'd suggest starting with a smaller rod and a smaller pass. Multiple passes are better.

Similar Threads

  1. 250EX Rocks!
    By Twisted Z in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 11-25-2015, 05:09 AM
  2. PowerArc 300
    By Shield Arc in forum Stick Welding (SMAW)
    Replies: 6
    Last Post: 11-19-2014, 12:28 PM
  3. Powerarc 140 on 208 vac
    By daverepair in forum Stick Welding (SMAW)
    Replies: 18
    Last Post: 05-16-2012, 04:24 AM
  4. New PowerArc 200
    By Tasha71822 in forum Customer Testimonials
    Replies: 6
    Last Post: 11-05-2011, 11:21 PM
  5. everlast rocks
    By onlyellis in forum Introduce Yourself
    Replies: 1
    Last Post: 11-04-2008, 12:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •