This is with a PP256, but specifically the cutter part.
Neighbor brought over a shaft off of his lawn mower, and just wanted the pulley off of it.
Another flange was in the way to get it on the press, so he wanted me to cut it.
So I cut it in one place, it started going through it like butter, but then hit a spot it would not cut. I would move the torch to the side, and it would cut fresh metal, but not this one spot. I moved down a inch, and cut through it in no time.
The shaft was about 3/4"
Any ideas?