    This is with a PP256, but specifically the cutter part.

    Neighbor brought over a shaft off of his lawn mower, and just wanted the pulley off of it.

    Another flange was in the way to get it on the press, so he wanted me to cut it.

    So I cut it in one place, it started going through it like butter, but then hit a spot it would not cut. I would move the torch to the side, and it would cut fresh metal, but not this one spot. I moved down a inch, and cut through it in no time.

    The shaft was about 3/4"

    Any ideas?

  2. #2

    Default

    Quote Originally Posted by Slick View Post
    This is with a PP256, but specifically the cutter part.

    Neighbor brought over a shaft off of his lawn mower, and just wanted the pulley off of it.

    Another flange was in the way to get it on the press, so he wanted me to cut it.

    So I cut it in one place, it started going through it like butter, but then hit a spot it would not cut. I would move the torch to the side, and it would cut fresh metal, but not this one spot. I moved down a inch, and cut through it in no time.

    The shaft was about 3/4"

    Any ideas?
    Hello Slick

    i will double check with the guys but it maybe a torch problem. If this is the case i will express you new one asap.
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  3. #3
    Join Date
    Jul 2010
    Location
    In the Land of CoRn
    Posts
    69

    Default

    Oleg,
    I doubt its the torch as it cut the shaft just fine if I would move it out of this area, and it cut all the way through it just a inch down.

    I didn't know if it was something I did, or what, just seemed odd, there was just this one spot of metal that wouldn't cut.

    Although the only consumables for plasma(actually period) that I have are what came screwed to the torch, thanks to UPS.
    Last edited by Slick; 08-12-2010 at 05:10 AM.

  4. #4

    Default

    Quote Originally Posted by Slick View Post
    This is with a PP256, but specifically the cutter part.

    Neighbor brought over a shaft off of his lawn mower, and just wanted the pulley off of it.

    Another flange was in the way to get it on the press, so he wanted me to cut it.

    So I cut it in one place, it started going through it like butter, but then hit a spot it would not cut. I would move the torch to the side, and it would cut fresh metal, but not this one spot. I moved down a inch, and cut through it in no time.

    The shaft was about 3/4"

    Any ideas?

    a plasma won't go through the rust so well, perhaps you had a large flake of rust.

  5. #5
    Join Date
    Jul 2010
    Location
    In the Land of CoRn
    Posts
    69

    Default

    No rust where I was cutting, but there was oil on the shaft that I cleaned off, but where is stopped cutting on the shaft was in the center.

  6. #6

    Default

    Slick,
    Unless there was a non conductive center or a shaft of grease...I can't think of any reason.

  7. #7
    Join Date
    Jul 2010
    Location
    In the Land of CoRn
    Posts
    69

    Default

    Quote Originally Posted by performance View Post
    Slick,
    Unless there was a non conductive center or a shaft of grease...I can't think of any reason.
    probably some non conductive material, thats all I can think of, the pulley ended up self destructing while pressing the shaft out anyway.

Similar Threads

  1. Cnc cutting with everlast 60s
    By FeddFab in forum Everlast Plasma Cutters (PAC)
    Replies: 7
    Last Post: 10-24-2013, 09:51 PM
  2. Anybody cutting 1"?
    By Jake98 in forum Everlast Plasma Cutters (PAC)
    Replies: 19
    Last Post: 05-11-2012, 06:19 PM
  3. DIY dryer for plasma cutting and TIG welding. Dross cutting or TIG electrode fur
    By everlastsupport in forum Welding articles from Professionals (knowledge database)
    Replies: 0
    Last Post: 03-15-2012, 01:08 PM
  4. Plasma Cutting
    By Lone Wolf in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 01-09-2012, 03:27 PM
  5. cutting at an angle
    By McClary in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 12-29-2011, 01:01 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •