I have a web site http://www.einstyn.com I make and sell chevelle parts.
this is the plates that get welded in to the control arms for stiffening. the plates are cut out of 1/8" steel with the plasma cutter. I use a thick aluminim template to guide the cutter tip to cut each piece the same quickly.
[img]http://www.einstyn.com/einstyn1/a-arm-2.jpg[/img]
I also make these pinion mounted parking disc brake. the bracket is cut with the plasma cutter as well.
[img]http://www.einstyn.com/einstyn1/p-brake10a.jpg[/img]