Originally Posted by
Tinman565
New here.
Just purchased a Lightning 275.
I find it odd (and I'd like your opinions and feedback) that Everlast cools the Dinse connector first... then the head of the torch.
We also own a Miller Syncrowave 350 and matching cooler... and Miller runs their flow the OPPOSITE way.
They cool the line and head first, then the Dinse connector and back out to the tank.
Which way is better and why ?
I'm guessing they could be run either way, but thought this was weird.
Anybody else have another brand that does it a certain way ?
Just curious.