any one using this PARKER SGP 360A PUSH-PULL GUN ?
seems that it would get hot on your glove. unlike a regular push pull gun
any one using this PARKER SGP 360A PUSH-PULL GUN ?
seems that it would get hot on your glove. unlike a regular push pull gun
Why would it? It is a REGULAR push pull. No more than a spool gun or anything else. A python type push pull gun get's hotter on your hand by design. Your hand is closer to the arc.
Mark