im welding 1/8" stainless plate to practice on. using 3/32 tun. and 3/32 filler rod @ 70 amps with pedal control hooked up, havnt spend much time dialing it in but welds seem dark and not pritty you could say, whats everyones settings to get started on something like this. also im on 110v about will have 220v in a couple days