Sorry, it's been a bit since I followed up on this issue. I have since tried 1/8" tungsten (1.5% Lanthanated) and I continue to have the same results. The end of the tungsten never obtains a smooth ball surface, instead, it ends up with tiny balls all over the end. I never set my balance above 30, and I typically run 25 - 28. Also, if I try different wave shapes, such as Triangular or Sine, the amperage is significantly lower than in Advanced Square setting. Not sure if this is normal. This applies to my 210EXT as well as 325EXT.