253 dDPI Inductance
Hi, The Manual for my 253DPI reads, (p33-4) that inductance can help with larger wire sizes on lighter materials. Which direction would it be adjusted for a larger than standard wire and, would it also apply to pulse operations the same? Thanks Edward
-
depending upon what wire you are using (metal type) it will vary. But typically it ranges between 3 and 5.