Share
Results 1 to 1 of 1

Thread: New PowerPro 256D Plasma air problem solved

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default New PowerPro 256D Plasma air problem solved

    Hi everyone,
    New to the Everlast Forum and happy new PowerPro 256D/ 375 Cooler owner.
    I had intermittent no air in plasma mode (code 806). tracked it back to the male quick connect nipple supplied with regulator/trap.
    The inner port was formed drilled so large (6mm) that the valve inside the Female quick connect fitting would slip inside and not be depressed and open the passage.
    AT TIMES! Some times would work for a few seconds and close, at times wouldn't open when connecting air hose. Aarrg!

    Quick repair. Silver Soldered port shut and re drilled to 3/16" All is well!

    Photos: Left nipple is Everlast supplied Right nipple is general stock part
    Would have changed nipples but Everlast supplied is straight thread w/o'ring and stock nipple is 1/4" npt.

    Hope this helps someone else if they have problems getting air from the Reg/trap.

    Regards,
    rbdeere318
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Everlast Nipple Before .jpg 
Views:	325 
Size:	148.0 KB 
ID:	14125   Click image for larger version. 

Name:	Everlast Nipple After.jpg 
Views:	325 
Size:	146.7 KB 
ID:	14126  