Share
Results 1 to 6 of 6

Thread: 210EXT does't weld. 804 error code

  1. Default 210EXT does't weld. 804 error code

    Has anyone any experience with error code 804?

    I started to weld aluminum, and the aluminum rod other end touched the metal table while I was welding and the TIG stopped working. Now It shows 804 in the display.

    Click image for larger version. 

Name:	Everlast_804_error.jpg 
Views:	392 
Size:	136.4 KB 
ID:	14121
    Click image for larger version. 

Name:	everlast_measuring.jpg 
Views:	427 
Size:	42.2 KB 
ID:	14122

    I measured the inverter and it doesn't work correctly. But it is very difficult to find the fault without schematics. Also the build "quality" is far from good. Many components are added afterwards on top of the other and so on.
    Click image for larger version. 

Name:	Everlast_quality.jpg 
Views:	383 
Size:	141.1 KB 
ID:	14123
    Click image for larger version. 

Name:	Everlast_quality2.jpg 
Views:	403 
Size:	133.8 KB 
ID:	14124

  2. #2

    Default

    That looks like an older 210? Call tech support at 877 755 9353 ext 207. They can help you. After you do, please report back.

  3. Default

    I bought it 2016, I don't know if it is "older" or not

    I sent email to support. They were guessing that the inverter board is broken. It indeed looks like it, but I want to be sure first before I buy spare parts.

  4. #4

    Default

    Check and see if you are still under the 5 year warranty.

  5. Default

    Unfortunately here in Finland we seem to have only two year warranty
    http://www.everlastwelds.fi/english/index.html

  6. Default

    I fixed it! One diode was broken from this board. I don?t know what it is for.

    Click image for larger version. 

Name:	C790EC21-BFE6-464A-A361-DE145752C07D.jpg 
Views:	460 
Size:	21.3 KB 
ID:	14127
    Click image for larger version. 

Name:	B75BC9AC-82A1-460C-8740-17E77539B123.jpg 