Has anyone any experience with error code 804?

I started to weld aluminum, and the aluminum rod other end touched the metal table while I was welding and the TIG stopped working. Now It shows 804 in the display.

Click image for larger version. 

Name:	Everlast_804_error.jpg 
Views:	387 
Size:	136.4 KB 
ID:	14121
Click image for larger version. 

Name:	everlast_measuring.jpg 
Views:	425 
Size:	42.2 KB 
ID:	14122

I measured the inverter and it doesn't work correctly. But it is very difficult to find the fault without schematics. Also the build "quality" is far from good. Many components are added afterwards on top of the other and so on.
Click image for larger version. 

Name:	Everlast_quality.jpg 
Views:	378 
Size:	141.1 KB 
ID:	14123
Click image for larger version. 

Name:	Everlast_quality2.jpg 
Views:	400 
Size:	133.8 KB 
ID:	14124