Thread: Super wide etching on Aluminum!

  1. #41

    Default

    Guys,(and ladies)

    IF you are due to receive a board, PLEASE call in and confirm your shipping address, again and make sure all is right with the unit at the same time otherwise. Even if you think we have it, please confirm again anyway. This will ensure flawless delivery to the correct address.

  2. #42

    Default Etching fixed

    Received the board and installed today. See before and after pictures. Works very well. The #5 or #7 refer to the gas lens cup size. Sequence was top to bottom. Thank you for fixing the issue.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	250ex new board v2.JPG 
Views:	407 
Size:	63.0 KB 
ID:	512  

  3. Default New boards

    Cool, can't wait to get mine! Thanx for posting the pics! How was the install? - Thx, Lou

  4. #44

    Default board replacement

    AC frequency board replacement.
    It is a small, about 3"x5" board located on the left side toward the front, just above center. Point of reference is standing in front of the machine looking at the control panel.
    Not that it is correct, my procedure:
    1. Shut it off, let it sit for awhile - let capacitors discharge.
    2. unplug
    3. move the machine so you can get to the 6 screws that go up through the bottom of the front and rear covers.
    4. remove the 4 screws (horizontal) that go through the front black plastic cover.
    5. repeat for the rear cap.
    6. remove the 3 screw (vertical) that go through the bottom of the front black plastic cap.
    7. repeat for the rear.
    8. remove the rear cap and handle.
    9. gently pull the front cap and control panel forward just enough to clear the metal case.
    10. remove the 10 screws that hold the metal case to the frame, 5 per side, 3 along the bottom, 2 just above center.
    11. gently left the case off the machine. Bend out a little so the vents will clear components.
    12. remove the 4 screws holding the circuit board to be replaced - left side toward the front, just above center. Point of reference is you looking at the control panel.
    13. pull the bottom of the board away from the machine. You will now have working room to swap the 6 plugs.
    14. swap the plugs, one at a time, board to board. Note: there are 6 plugs to swap. There are 7 connectors on the board. Some connectors can be plug into more than one location.
    15. reverse the above.
    16. Be careful not to pinch wires on the left side.
    16. Don't forget to the handle back in before securing the back cap - not that I forgot.

    Not hard, just use a good #1 Phillips and take you time.
    Last edited by dlong; 09-05-2010 at 02:31 AM. Reason: Meant to say AC Balance board replacement

  5. #45

    Default

    If I remember right, front panel removal is not necessary.

Similar Threads

  1. Super Ultra ?
    By fitter in forum Pre-sales, Sales and Shipping questions
    Replies: 8
    Last Post: 04-29-2013, 10:58 PM
  2. wide etching on aluminum
    By johnson697 in forum General Welding Questions
    Replies: 28
    Last Post: 11-25-2012, 02:33 PM
  3. super cut 50p
    By johnnie in forum Everlast Plasma Cutters (PAC)
    Replies: 7
    Last Post: 11-11-2012, 12:51 AM
  4. Super Cut 50P HELP.
    By shrop3 in forum Everlast Plasma Cutters (PAC)
    Replies: 9
    Last Post: 02-04-2012, 02:08 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •