Hello, Wondering if there is a spray bomb paint match that is close to the green? Paint on the case is really flaking, bubbling up. They need to doma better job on prep before the paint.
Hello, Wondering if there is a spray bomb paint match that is close to the green? Paint on the case is really flaking, bubbling up. They need to doma better job on prep before the paint.
Gee,
I've never before heard anyone complain about the paint finish on an Everlast unit.
I mean, my 210EXT is still brilliant and unblemished after 6 years.
I'm pretty sure they're all powder-coat/baked on.
I even took a car buffer to get the Everlast trade name portion off mine, and put my YouTube Channel url on the side for a while. But I think YouTube is shadow banning my Channel a bit, so I'm looking to migrate away from YouTube as a platform.
Anyway, post up a pic or two of your unit.
Otherwise, why not just refresh the paint finish completely, with a color of your pick.
I mean, I like how the AHP TIG units have no louvered vents on the side panels, so that their whole sheetmetal could be remade with aluminum diamond-plate. I've seen one or two examples of that having been done, and it's way-cool!
I have a little metal brake that can do simple bends of .100 aluminum to about 20" wide, so I've been tempted to make a diamond-plate cover for my 210EXT, but I'd probably want to get a louver-punch jig ($$$) to do it in an aesthetic and elegant way.
Last edited by christian; 01-21-2021 at 10:17 PM.
If its fairly new, call and ask about warranty on the cover.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
This one is out of warranty. Paint is bubbled and peeling all over. Was just inquiring if someone else has found a close match. I’d have to do the cooler as well if I paint another color. I can have it computer match.Just have to cough up the cash. Are decals available to replace the stock ones which will be gone if I repaint?
Its RAL 6018. We've put that paint code on here somewhere.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Thanks for the code! Are there any “ Everlast” decals or stickers available?
No. This is screen printed on.