Help: lightning MTS 275 not feeding (video)
Hey everyone, noob here. I'm attempting to feed some 0.035 ER 70S-6 wire through my new Lightning MTS 275. This is its maiden voyage, never used it before. The feed rollers are turning off by themselves after a second. Seems almost like some form of safety shutoff or something like that.
- The drive rollers are tensioned near the lowest setting
- The spool rotates fairly freely, but doesn't spin very much at all if I give it push
Video: https://youtu.be/c4AR21rBYvM