    Evening - I recently purchased a 275p I-MIG unit and it resides in my attached garage which isn't heated.
    Is there a temperature range in the specs that I can't seem to find, that recommends how low of a temperature that Everlast welders can or should be used in?
    Up here in Northern Canada - we can get down often into the low -40 degree range and I'm not likely going to be out in the garage doing any welding at that point!
    But do Everlast welders have a temperature range that a unit like a 275p should be limited to?
    For example - tonight will be close to 0 degrees C or 32 F for you non-metric guys - is it advisable not to fire up such a welder and use it at that temperature or even below that?
    I often put a portable heater and warm up the area where this new welder will reside, often up into a decent range to do odd jobs, to the point where I consider it quite comfortable - probably into the mid 40 to 50 Fahrenheit levels, which I assume would be no problem - but it would be nice to know if there are there any real limitations to try and adhere to.
    Thanks!

  2. #2

    Default

    14 to 104 F operation. Storage at 40 below is not recommended.

  3. Default

    Thanks very much!
    My garage never cools down enough to freeze cans of soda or even small water bottles so I guess I'm somewhat OK - but maybe pushing it still.. as the fans might make the internals think it is 32 F or cooler with the air flow.