As title specifies

Recommended tungsten prep

2% EWLa 1/16th Dia.

Whats crackin? I am new to the forum and made an intro post in the Intro section.

I am getting back into welding after 11 years of QC and R&D work with GMAW. Its been many moons since I hit a real lick welding aluminum. I picked up a 255 Ext and so far am impressed with the current DC only use. I have been attempting to run some 1/16th Tungsten and get erratic results with it "balling" up. I initially had some that were sharpened way to sharp and backed off to a 30 degree prep and a blunted point.

120hz AC, Square wave. 40% EP ~50-60 amps max current.

Would leaving the electrode square cut be a better prep.

I did do a search and did not seem to find a related post or topic.

If there is one then please link and I will read away.

Regards.

Jeb.