    We have a pedal and the torch upgrade. This system has a 3" Magnaflow muffler, stainless flex pipe, 3 exhaust band clamps for easy removal and is 3" from front to back over the axle and a 3" to 4" end cap. We tacked the system for fit up on the car and now we're trying to get a real nice look on the welds. My grandsons are inheriting the shop and want to build high performance engines (too new for me). We build engines and transmissions now and have a full paint shop. They learn quick and are "tech" savvy (I'm not).

  2. Default

    Yeah,

    Nice looking welds will most likely happen on the bench, with a bit bigger cup, more Argon flow, some back-purging, along with a lot of stainless TIG welding experience.

    Or, like I did, as a newbie, none of that, and just some flap disc action to get a seamless look to hide the unflattering bead appearance. Ha, ha, ha... I mean, I could have brushed-out those beads with a wire wheel to make them look OK, but I knew I'd probably want the nicer seamless look.

    But, it would be nice to see a pic of the layout, fit-up, and tack-up, i.e., how many actual welded joints there'll be.

    Otherwise, that 161STH seems to have a Pulse feature, which may help control your heat input, especially with no Pedal. So, try some practice pieces with Pulse.


    Quote Originally Posted by TNDoug View Post
    We have a pedal and the torch upgrade. This system has a 3" Magnaflow muffler, stainless flex pipe, 3 exhaust band clamps for easy removal and is 3" from front to back over the axle and a 3" to 4" end cap. We tacked the system for fit up on the car and now we're trying to get a real nice look on the welds. My grandsons are inheriting the shop and want to build high performance engines (too new for me). We build engines and transmissions now and have a full paint shop. They learn quick and are "tech" savvy (I'm not).
    Last edited by christian; 05-24-2020 at 02:41 AM.
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  3. #3

    Default

    We use a mig welder a lot in the shop for body work. We're set up to back purge so we'll see how it goes. The "boys" have better hand/eye co-ordination so they'll figure it out. Thanks for the input, sounds like we're headed in the right direction.

  4. #4

    Default

    Are you using pure argon?

  5. Default

    Gee,

    Here's a new Everlast video from their YouTube Channel which happens to be on stainless exhaust TIG welding, and how much difference back-purging makes.

    .035 filler, too.

    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  6. #6

    Default

    You said you didn't back purge, now you're for it? For the record, I said I back purge. I've already seen this video. You don't seem to be offering any new information. Thanks anyway.

  7. Default

    Yeah,

    I said I was naive back then.

    So, I do now recommend back-purging, especially if it?s for a commercial customer.

    I might be able to offer some better or more helpful input, if you?d provide some feedback in the form of a pic of the system layout, the fit-up, tack-up, how many welded seams, etc?

    A pic can tell a lot.

    Are you considering Pulse, then?
    Last edited by christian; 05-25-2020 at 03:32 AM.
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  8. #8

    Default

    Yep. Pure Argon.