hello everyone, my first TIG machine and new to TIG. I set everything, got my 100% argon. I have the following so far....

#6 cup with a 1/16 Tungsten
Pressure gauge is at 12 psi
I have it set at 80 amps to play around with some steel
2T setting
I am using the hand control for now so I can learn it because I would like to do some tig work INSIDE my car where a foot pedal would be impossible to use.

Any tips and help would be appreciated it. I have been watching youtube videos as well and browsing this forum