Up front this is probably 100% operator error, but I can't seem to figure it out so I need your input.
POWERTIG 200DV
I have been trying to weld aluminum. Cannot get an arc, just seems like many random lightning dots in the torch area and cannot even get a puddle to form, also leaving tiny pock marks in the material.
3/16 by 1" bar, just for practice. Everything is super clean. Reground the tungsten a hundred times. Furick #10 cup 3/32 tungsten gas turned way up.
Following all the tips favoring more heat and penetration.
FINALLY at frequency 220, balance 30, power all the way at 200, trying for the hundredth time, the arc started with a pop and I got a huge cone and it flat melted everything in its path very quickly.
So now I am satisfied it's suddenly functioning correctly, I obviously have to scale the power and frequency down.
Unfortunately I don't have any more aluminum to try on, this was my last test piece, going to have to buy some more bar at work next week.
My question is what was I doing wrong? Why did the arc suddenly form correctly? Why did it do the crazy shotgun arc thing for so long before it decided to behave?
Please help me learn.