 Originally Posted by 
performance
					
				 
				That wasn't me that said that about the 75/25.  I respect Zoama.  I've done it with it, but there is no comparison, and so many more problems and much less stability.  I said 80/20, which is recognized as the lower threshold.  Personally, I use a C18. This is a good mix for both spray and short circuit, and you get a cleaner weld in short circuit.   It's not as hot, but it works wonders in spray too.  For spray it does run a bit hotter than 90/10, but it does offer true spray capability.  Let's put it this way, you can spray with a lot lower settings with 90/10 instead of 75/25.