The first time I TIG on AC the pre-flow works but subsequent welds the arc starts immediately without any pre-flow. Any ideas?
Thanks
Don
							
						
					
					
						The first time I TIG on AC the pre-flow works but subsequent welds the arc starts immediately without any pre-flow. Any ideas?
Thanks
Don
Gee,
It may be possible that you're just reinitiating a subsequent arc start while the post flow is still going, so you're not hearing any newly initiated pre-flow starting, i.e. if your post-flow is at 20 sec, turn it down to about 5 sec.
I usually only set for about .5 sec of pre-flow, if at all.