Hello Everyone...............
According to specs, the 140E can do .35 wire. I bought a roll and some tips recently and trying on 12g steel, couldn't find the bacon anywhere.
1st.. I'm new to welding so it may factor in but I have no problem finding the sound when using .23 / .30 wire
2nd.. I use the wife's washing machine outlet when welding. It's 120 on a 20amp breaker.
I understand that to get the best performance I should be on a 30amp breaker.
Question: Unless I constantly trip the 20amp breaker (which I haven't yet) is there really a need to go with 30amps since I don't think I'm loading the machine.
As when using the .35 wire on the 12g steel, I went up and down both dials but never found a stable sound. I was grounded to the work and not the table. I used a flapdisk to clean the steel and then used cleaner and a clean rag to wipe it down. I use 75/25 gas and it was set to 20-25.
As in #1 above it may be operator error but I think I covered all the bases. And since I wasn't trying to weld up a Sherman tank body I figured that the 140 would be able to run the .35.
Thanks Gordon




Reply With Quote