I'm looking for advise on practice drills. I well be using my 225LX on very small steel fire arms parts, building up worn areas. Some of these parts are 180 years old.
Should I start with a 1/16 or 1/8 2% Thoriated tungstens? What would be a good filler rod? I was thinking of using 1/16 ER70S6.