  1. Default Just getting started

    I'm looking for advise on practice drills. I well be using my 225LX on very small steel fire arms parts, building up worn areas. Some of these parts are 180 years old.

    Should I start with a 1/16 or 1/8 2% Thoriated tungstens? What would be a good filler rod? I was thinking of using 1/16 ER70S6.

  2. #2

    Default

    The 3/32 is the best all around tungsten for most general welding. But as a gunsmith, you may need to consult some tech manuals on gun repair to identify the best combination of amps and tungsten, as well as filler material. 70s6 is a very good all around rod, with high silicone content for deoxidizing.

Similar Threads

  1. Looking for advice on getting started with a 200DX
    By EmptyNester in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 12-10-2012, 01:01 AM
  2. PP 205 Setup and getting started.
    By qcksnake in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 12-30-2011, 02:40 AM
  3. My wife started talking about plasma cutters last night.
    By Haywire in forum Everlast Plasma Cutters (PAC)
    Replies: 13
    Last Post: 05-15-2011, 02:20 AM
  4. Started my plasma table today.
    By A/C Guy in forum Other Custom Fabrications
    Replies: 13
    Last Post: 04-12-2011, 02:00 PM
  5. just getting started
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 03-03-2011, 02:04 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •