Quote Originally Posted by 3goutdoor View Post
I was inquiring about a footpedal to a vendor for the 141 STL (not Everlast) and in discussion I said they-everlast- recommended a 22 ohm nova pedal. And I said by the way I have one of your 47ohm pedals for a different machine. And he says I should try the pedal and see how it works on the 141. Bought with pp205s. Is there any harm in trying and see the results or will a different ohm foot pedal harm the machine?
No problem, there will just be a slight difference in the rate the amps change. You probably won't even be able to tell the difference.