Share
Results 1 to 6 of 6

Thread: 250 EX Foot pedal

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1
    Join Date
    Aug 2014
    Location
    Burnsville, Minnesota
    Posts
    4

    Post 250 EX Foot pedal

    I purchased a Everlast TIG welder POWERTIG 250EX about two years ago. I have been very happy with it so far except for the foot petal. It is far to sensitive. The unit came with a FT-22-CL. I measured the resistance across pins 3 and 5 of the connector and read approximately 20 kohms. Would it be possible to take the foot petal apart and replace the potentiometer with 50 kohm linear potentiometer of the same type. Would there be any other advantages to order a new EV-PowerPedal-50DL.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Dick Eue View Post
    I purchased a Everlast TIG welder POWERTIG 250EX about two years ago. I have been very happy with it so far except for the foot petal. It is far to sensitive. The unit came with a FT-22-CL. I measured the resistance across pins 3 and 5 of the connector and read approximately 20 kohms. Would it be possible to take the foot petal apart and replace the potentiometer with 50 kohm linear potentiometer of the same type. Would there be any other advantages to order a new EV-PowerPedal-50DL.
    The pot is wired as a voltage divider, so changing the value will not have that much effect. However, changing the taper from linear to log or vise versa will. You can also get reverse log, if you want that. The quality of the pot also has a big impact on smoothness of current transition. So be sure to get a good one. To get the most resolution set the panel at the expected max current or just above, that way you have the most response from the pedal, as well.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Quote Originally Posted by Dick Eue View Post
    I purchased a Everlast TIG welder POWERTIG 250EX about two years ago. I have been very happy with it so far except for the foot petal. It is far to sensitive. The unit came with a FT-22-CL. I measured the resistance across pins 3 and 5 of the connector and read approximately 20 kohms. Would it be possible to take the foot petal apart and replace the potentiometer with 50 kohm linear potentiometer of the same type. Would there be any other advantages to order a new EV-PowerPedal-50DL.
    Do you have the black rocker switch?

  4. #4
    Join Date
    Aug 2014
    Location
    Burnsville, Minnesota
    Posts
    4

    Post

    Quote Originally Posted by performance View Post
    Do you have the black rocker switch?
    I'm not sure what the black rocker switch is or where it is so maybe I don't have one.

  5. #5
    Join Date
    Aug 2014
    Location
    Burnsville, Minnesota
    Posts
    4

    Post

    Quote Originally Posted by Dick Eue View Post
    I'm not sure what the black rocker switch is or where it is so maybe I don't have one.
    Do you mean the torch switch?

  6. #6

    Default

    On the front of the control panel, You have a row of rocker switches to select modes, or you have a row of green touch buttons that do the same thing.

Similar Threads

  1. Foot Pedal Bottom Pad
    By NRM in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 17
    Last Post: 08-22-2012, 10:46 PM
  2. Foot Pedal Fix
    By Ron66 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-26-2012, 12:29 AM
  3. new foot pedal
    By hesstx in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 12-16-2011, 05:26 PM
  4. Bad foot pedal?
    By sth212 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 08-21-2011, 08:50 PM
  5. Old Foot Pedal
    By McClary in forum TIG Welding (GTAW/GTAW-P)