    Been doing a bunch of pulse welding with my brand new 255EXT on round aluminum tube to dial in the best settings. Everything was going great laying down some excellent beads. All of sudden it changed sound and seem like it wasn't giving me the same amps. Welding at 205 amps, took my helmet off and floored it and it will only give me about 75 to 100 amps on the hot side (welding amps) of the pulse??? Shut of the pulse and floored it and goes right up to the 205 amps I have it set at. Any thoughts? All of my work is on a positioner with stationary torch holder for consistency so everything is the same every time.
    1/8" 2% Lanthenated tungsten sharpened to a point
    12 to 15 CFH
    3/32 4043 filler rod
    Last edited by travis1693; 09-20-2018 at 12:36 AM.
    Everlast 255EXT
    Everlast Water Cooler
    Pro-Arc weld positioner (Arc-Zone)
    Arc-Zone adjustable Tungsten Grinder
    Jet 7x12 horizontal/vertical bands
    Precision Matthews 950V Mill
    Grizzly GO4003 Gunsmith Lathe

  2. #2

    Default

    Travis,
    How long have you had it? The display on that unit IIRC averages the welding amps based off the pulse settings. But call 877 755 9353 ext 207 tomorrow. There is probalby a simple fix. I'd unplug it, take the cover off and reseat all the connectors. Allow it to sit for 15 minutes first.

  3. #3

    Default

    Quote Originally Posted by performance View Post
    Travis,
    How long have you had it? The display on that unit IIRC averages the welding amps based off the pulse settings. But call 877 755 9353 ext 207 tomorrow. There is probalby a simple fix. I'd unplug it, take the cover off and reseat all the connectors. Allow it to sit for 15 minutes first.
    Mark,
    I've only had it about 11 days. I gotta say man before this happened, I was VERY IMPRESSED with the 255. I am by no means and expert on Aluminum TIG, but it's night and day better than my Lincoln, (last time I will use that fowl language on here LOL). Having the ability to dial in both sides of the pulse and the time the pulse remains on the welding amp side is just simply amazing.

    I agree with you that its probably nothing major wrong just something simple.
    Thank you for giving me the number I will give a call, get it figured out and share my results.

    Thanks again,
    Travis
    Everlast 255EXT
    Everlast Water Cooler
    Pro-Arc weld positioner (Arc-Zone)
    Arc-Zone adjustable Tungsten Grinder
    Jet 7x12 horizontal/vertical bands
    Precision Matthews 950V Mill
    Grizzly GO4003 Gunsmith Lathe

Similar Threads

  1. 200DX, what am I doing wrong?
    By rappy'97 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 09-08-2015, 11:59 AM
  2. New Everlast Pulse on Pulse Machines?
    By m10za in forum Pre-sales, Sales and Shipping questions
    Replies: 3
    Last Post: 02-04-2015, 07:53 PM
  3. Wrong part
    By dsmabe in forum Pre-sales, Sales and Shipping questions
    Replies: 17
    Last Post: 07-17-2014, 07:57 PM
  4. What am I doing wrong???
    By Toby in forum TIG Welding (GTAW/GTAW-P)
    Replies: 36
    Last Post: 04-09-2013, 12:54 AM
  5. wrong helmet sent
    By bubbas55 in forum Pre-sales, Sales and Shipping questions
    Replies: 1
    Last Post: 12-01-2012, 08:21 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •