    Im trying to do outside corner welds on .063 or so aluminum. I suck at it. Im not building anything. just trying to stick 2 pieces of aluminum together in a respectable manner.
    IF I can get a puddle without melting the edges, as soon as I approach with the filler, the arc starts wandering, and sounds like popcorn. And the filler drips onto the aluminum. I havent dipped the tungsten or touched it with the filler. Im reasonably certain i've prepped the tungsten properly,(longitudinal grinding on a dedicated wheel etc..) and everything is cleaned with a dedicated brush and acetone. im using 1/16 blue or purple tungsten ,powerpro 164 welder, various gas flows from 7-15 lpm of 100% argon,#8 cup, various amp settings from 35 -100. usually around 60.
    Did I leave anything out?
    Thanks, John
    שלום

  2. Default

    Gee,

    With thinner stuff like that, I'll guess that your arc is too long, and it smokes your filler before it gets to the puddle, even with mild amperage.
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  3. Default

    Thanks, will too long of an arc make it sound like popcorn popping?
    שלום

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    If you haven't dipped the tungsten, you probably aren't close enough. A good rule of thumb is to hold an arc length no more than 1 tungsten diameter.
    1/16" (1.6mm) material is a little tricky. You might want to start with double that thickness then work down once you get the hang of it. Also some kind of chill bar or other heatsink can go a long way to keeping things under control. Another good practice is to just do some edge buildup welds on thin material before progressing to joints. It helps to use filler smaller than your material thickness. 1/16" filler is great for welding 1/8" plate, but for 1/16" plate, it can be a little much. You might want to try some .045" or .035" to keep from adding too much with each dab.
    Long arc, short arc, heliarc and in-the-dark!

  5. Default

    Yeah,

    Touching filler directly on the tungsten, rather than dipping the tungsten in the puddle, can also give you "popcorn". Ha, ha, ha...

    The tungsten must be re-ground each time, to have any real chance of a good result going forward.

    If you're not seeing the arc and puddle very well, I suggest that you get a good, adjustable welding lid.

    Quote Originally Posted by JohnT View Post
    Thanks, will too long of an arc make it sound like popcorn popping?
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

  6. Default

    thanks guys, ill keep plugging away at it
    שלום

Similar Threads

  1. New to welding. Which filler rod?
    By Xman4u in forum General Welding Questions
    Replies: 2
    Last Post: 01-16-2015, 11:43 AM
  2. Where to buy magnesium tig filler rod???
    By Brian Ski in forum General Welding Questions
    Replies: 12
    Last Post: 04-17-2014, 06:41 PM
  3. Using MIG wire for TIG filler.
    By blasphemy000 in forum General Welder Questions
    Replies: 6
    Last Post: 10-11-2011, 01:17 AM
  4. USING FILLER ROD Poll
    By Titan winch in forum General Welder Questions
    Replies: 16
    Last Post: 08-30-2011, 11:08 AM
  5. TIG Filler
    By bigjoeinkg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 07-18-2011, 09:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •