    Yeah,

    I wouldn't sweat that stuff at the outset, especially since small coupons aren't really representative of what an actual aluminum project is like, i.e., they saturate heat quickly, so each bead is not equal in heat input and amperage adjustments. So, that's why it can seem like you start with too much heat, because of preheat or heat saturatation, which is abnormal. The norm is for the beginning of a bead or a seam to be a tad cold, then to call for some tapering off of the amperage toward the end.

    So, I'll suggest that you stop padding beads on plate. You're already doing well enough with that.

    Learn to tack aluminum quickly, effectively, and efficiently for about an hour.

    Then start with butt joints, lap joints, T-joint fillets, inside-corner joint fillets, then outside corner joints.

    That could take about a week in some spare time, with maybe a bottle or two of Argon.

    Then, if you come back to pad some beads, it'll be easier.

    I relied on the Triangle wave, 1/16" filler, and about 200 Hz on AC frequency for outside-corner joints with thinner aluminum for a while, because I like a smaller, narrower beads, even on outside corners. But, often a Squarewave and a lower AC frequency, with a 3/32" filler may be prefered by some, to wrap the corners better and have more metal deposition. And I'm tending to ween myself off of the Triangle wave some now. But I still like to keep a higher AC frequency on most everything. And don't bother to use the Triangle wave for inside corner fillets, as the Squarewave brings more heat with it, which inside corners call for, but higher AC frequency is still good on them.

    Yeah, a blue or purple tungsten tip is a sign of too short a post-flow.

    Getting into a comfortable position is big for me. And I try to prop my torch hand as well as my filler hand, whenever possible, as I'm not a rock steady TIG welder to begin with. Butted, notched, round tubing fillets seem the most challenging for me, I guess.

    So, yeah, you're smokin' dude.

    Time to move ahead already!

    Quote Originally Posted by elcamino View Post
    thank you christian, i will work on it and keep at it. anything else you can see that can help? i think i was starting with to many amps on some beads they are wide and flat and others not enough because they were higher and narrower?

    regarding the post flow not being long enough, is the reason why the tungsten turns blue after a bead?
    Last edited by christian; 04-04-2018 at 01:56 AM.
    Everlast 210 EXT (2015)

    www.youtube.com/newjerusalemtimes

Similar Threads

  1. First Time to TIG Aluminum Problems
    By gtty in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 10-07-2014, 12:52 AM
  2. First time welding cast aluminum
    By Ron66 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 10-28-2012, 02:39 PM
  3. Replies: 23
    Last Post: 05-23-2012, 05:17 AM
  4. Replies: 9
    Last Post: 09-08-2011, 11:57 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •