Thread: Preheating in an oven

  1. Question Preheating in an oven

    So here is the next in my long list of stupid welding questions.

    200e running on a 30 amp 110 volt circuit.

    I am going to weld up a trailer hitch insert...so the part the ball sits on. I have scrap 1/2" angle iron and the 1/4" thick tube that I'm using.

    I've done half inch stuff before with an even wimpier 110v welder, but I set that on a propane burner long enough to turn a dull red. It worked quite well.

    I am considering putting these bits of metal in the oven on broil (500F) for an hour or so (since I don't have the propane torch anymore) then do the welding.

    Am I wasting my time by doing this?

    Is the 200e more than powerful enough to handle 1/2"?

    thx

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    A little preheat is always nice, but the real thing is to bevel the joints properly and do multi pass welds.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Preheating to help Stick Welding
    By undercut in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 05-07-2012, 07:30 PM
  2. two dollar rod oven
    By geezer in forum Stick Welding (SMAW)
    Replies: 20
    Last Post: 01-22-2012, 01:57 PM
  3. Powder Coating Oven project
    By DAC45 in forum Other Custom Fabrications
    Replies: 19
    Last Post: 10-13-2011, 04:18 AM
  4. Powder Coating Oven
    By acourtjester in forum Other Custom Fabrications
    Replies: 4
    Last Post: 07-01-2011, 08:59 PM
  5. Got my eye on a small rod oven
    By Haywire in forum General Welding Questions
    Replies: 8
    Last Post: 06-10-2011, 09:06 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •