Thread: Preheating in an oven

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Question Preheating in an oven

    So here is the next in my long list of stupid welding questions.

    200e running on a 30 amp 110 volt circuit.

    I am going to weld up a trailer hitch insert...so the part the ball sits on. I have scrap 1/2" angle iron and the 1/4" thick tube that I'm using.

    I've done half inch stuff before with an even wimpier 110v welder, but I set that on a propane burner long enough to turn a dull red. It worked quite well.

    I am considering putting these bits of metal in the oven on broil (500F) for an hour or so (since I don't have the propane torch anymore) then do the welding.

    Am I wasting my time by doing this?

    Is the 200e more than powerful enough to handle 1/2"?

    thx

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    A little preheat is always nice, but the real thing is to bevel the joints properly and do multi pass welds.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Preheating to help Stick Welding
    By undercut in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 05-07-2012, 07:30 PM
  2. two dollar rod oven
    By geezer in forum Stick Welding (SMAW)
    Replies: 20
    Last Post: 01-22-2012, 01:57 PM
  3. Powder Coating Oven project
    By DAC45 in forum Other Custom Fabrications
    Replies: 19
    Last Post: 10-13-2011, 04:18 AM
  4. Powder Coating Oven
    By acourtjester in forum Other Custom Fabrications
    Replies: 4
    Last Post: 07-01-2011, 08:59 PM
  5. Got my eye on a small rod oven
    By Haywire in forum General Welding Questions
    Replies: 8
    Last Post: 06-10-2011, 09:06 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •