Share
Results 1 to 6 of 6

Thread: Mig Welding Perameters

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Mig Welding Perameters

    Does anyone have some good settings for your Everlast machine from 1/8th" up to 1/2" regular mild steel. I know a lot of variables go into it, just looking for some good starting points. I use to use an app on my phone my Lincoln and the setting seemed to be pretty close. However, after replacing my phone I can no longer find the app. I've tried the Miller app and the wire feed speed seems to be way off, unless it is my inexperience and i'm not moving fast enough. But I seem to get a better looking weld when I slow it down. I'm running a 251si in standard mig mode.

    For example the miller app states for 1/8th" using .35 wire I would be at 280-300 ipm and 18-19 volts

    When I weld at those settings I can feel the wire tapping the metal that I am working on.

  2. #2

    Default

    No one's settings are right even for their own brand machines. They are a loose guide. Very loose. The way you should set it is by what you hear, and what you see in the puddle. If you don't know what to look for, or don't know how it should sound, there are videos online that can help. You need to be able to see the puddle and recognize the puddle, and act accordingly. You can't auto pilot MIG. You still have to know what the puddle looks like, and what a proper arc sounds like. The only way to do this, is to practice, practice and practice...and watch GOOD videos on MIG welding.

  3. #3

    Default

    The Lincoln app is better to me. But I think it is still available. I downloaded one not long ago. Just search free welding apps. It should be there.

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by performance View Post
    The Lincoln app is better to me. But I think it is still available. I downloaded one not long ago. Just search free welding apps. It should be there.
    The Lincoln app seems to be gone. Now replaced with the Lincoln Library, and there seems to be a lot of complaints that they did not include the old parameter selector. The one thing I didn't like about the Lincoln one, was that they used their own product numbers not the industry standard designation. For example SuperArc® L-56® instead of ER70S6. And the one thing all the calculators seem to suffer from, is they don't include the travel speed. That has a huge impact on settings.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5

    Default

    I had downloaded both at the same time, and they were separate apps. Looks like it is not up now. hmmm.

  6. #6

    Default

    Google image search any manufacturers mig settings to see the door charts.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •