Evolution cold saw???
Anyone ever use one??? I never heard of evolution before, but sounds like they are out there. I was wanting to pick up a chop saw and ran across the cold saws (ones that use a steel blade instead of a abrasive blade.) The biggest problem is the cold saw blades are expensive. Starting price is about $400 and go way up. The Rage 2 had a price close to $300 a few years ago and now I see them on sale for under $200. Blades are expensive, but they last a lot longer than abrasive blades, as long as you are easy on them. Most damage is from forcing the cut. A lot less mess and cleaner cut than a abrasive blade. The reviews are considerably better than abrasive saws.
I can't find anyone who stocks them. Order only.
Rage 2
Brian... Still lurking in corners...
Shade tree MIG welder.