I had big plans this weekend to get caught up on projects, but no joy. I went to use the plasma cutter and the high frequency pilot arc did not work, I tried the TIG - no high frequency there either. I can start the both the plasma and TIG by scratching.
Its been about 3 weeks since I last used the machine and its unplugged when not in use. Machine was purchased new in April, is there anything I can do to fix it?
Thanks,
Tony